Multibase Multi-Flex® TPO 4107 BLK

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Olefinic Elastomer (TPO)
Manufacturer Multibase
Trade Name Multi-Flex® TPO
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multi-Flex® TPO 4107 BLK.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by Multibase.
Physical Properties Metric English Comments
Density 0.870 g/cc
0.0314 lb/in³
ASTM D792-91
Mechanical Properties Metric English Comments
Hardness, Shore D 41
41
10 sec; ASTM D-2240-95
Tensile Strength, Ultimate >= 11.0 MPa
>= 1600 psi
ASTM D638-95
Elongation at Break >= 50 %
>= 50 %
ASTM D638-95
Flexural Modulus 0.0600 GPa
8.70 ksi
Secant 1%; ASTM D-790-95