Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Multibase Multi-Flex® TPO D-3120

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Olefinic Elastomer (TPO)
Manufacturer Multibase
Trade Name Multi-Flex® TPO
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multi-Flex® TPO D-3120.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Multi-Flex® TPO D-3120 is a compound for automotive applications replacing Himont's 7023. The burn rate is 0.87 in/min; ASTM FM VSS 30.Data provided by Multibase.
Physical Properties Metric English Comments
Density 1.17 g/cc
0.0423 lb/in³
ASTM D792-91
Melt Flow 20 g/10 min
20 g/10 min
(Condition L) ASTM D-1238-94a
Mechanical Properties Metric English Comments
Hardness, Shore D 31
31
10 sec; ASTM D-2240-95
Tensile Strength, Ultimate 5.60 MPa
812 psi
ASTM D638-95
Elongation at Break 575 %
575 %
ASTM D638-95
Flexural Strength 4.50 MPa
653 psi
ASTM D955-89
Flexural Modulus 0.110 GPa
16.0 ksi
Method 1, Proc. B; ASTM D-790-95
Tear Strength 48.1 kN/m
274 pli
ASTM D624-95