Material Notes:
Data provided by Multibase.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D792-91
Linear Mold Shrinkage 0.013 cm/cm
0.013 in/in
ASTM D955-89
Melt Flow 10 g/10 min
10 g/10 min
(Condition L) ASTM D-1238-94a
Mechanical Properties Metric English Comments
Hardness, Shore D 65
65
10 sec; ASTM D-2240-95
Tensile Strength, Ultimate 19.3 MPa
2800 psi
ASTM D638-95
Elongation at Yield 20 %
20 %
ASTM D638-95
Flexural Modulus 0.0900 GPa
13.1 ksi
Method 1, Proc. B; ASTM D-790-95
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 70.0 °C
158 °F
ASTM D648-95
Brittleness Temperature -43.0 °C
-45.4 °F
ASTM D746-95