Material Notes:
Data provided by Multibase.
Physical Properties Metric English Comments
Density 1.17 g/cc
0.0423 lb/in³
ASTM D792-91
Melt Flow 8.0 g/10 min
8.0 g/10 min
(Condition L) ASTM D-1238-94a
Mechanical Properties Metric English Comments
Hardness, Shore D 64
64
10 sec; ASTM D-2240-95
Tensile Strength, Ultimate >= 15.2 MPa
>= 2200 psi
ASTM D638-95
Elongation at Break >= 100 %
>= 100 %
ASTM D638-95
Flexural Modulus >= 1.103 GPa
>= 160.0 ksi
Secant 1%; ASTM D-790-95
Tear Strength 93.0 kN/m
531 pli
ASTM D624-95