Material Notes:
Multi-Pro 2518 CU is a mineral reinforced polypropylene compound offering overall balanced impact and stiffness properties. This material is specially formulated with UV stabilization for outdoor exposure and is particularly suited for lawn furniture applications.Data provided by Multibase.
Physical Properties Metric English Comments
Density 1.08 g/cc
0.0390 lb/in³
ASTM D792-91
Linear Mold Shrinkage 0.0090 cm/cm
0.0090 in/in
ASTM D955-89
Melt Flow 18 g/10 min
18 g/10 min
(Condition L) ASTM D-1238-94a
Mechanical Properties Metric English Comments
Hardness, Shore D 72
72
10 sec; ASTM D-2240-95
Tensile Strength, Ultimate 24.1 MPa
3500 psi
ASTM D638-95
Elongation at Break 150 %
150 %
ASTM D638-95
Flexural Modulus 1.724 GPa
250.0 ksi
Method 1, Proc. B; ASTM D-790-95
Izod Impact, Notched 0.530 J/cm
0.993 ft-lb/in
ASTM D256-93a
Gardner Impact 5.60 J
4.13 ft-lb
ASTM D5420-93
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 102 °C
216 °F
ASTM D648-95
Deflection Temperature at 1.8 MPa (264 psi) 63.0 °C
145 °F
ASTM D648-95
Optical Properties Metric English Comments
Gloss 72 %
72 %
ASTM D2457-90