Material Notes:
Forms: PelletsInformation provided by Multibase
Physical Properties Metric English Comments
Specific Gravity 1.08 g/cc
1.08 g/cc
ASTM 792
Melt Flow 2.68 g/10 min

@Load 2.16 kg,
Temperature 230 °C
2.68 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 50.3 MPa
7300 psi
ASTM D638
Elongation at Break 16 %
16 %
ASTM D638
Flexural Strength 68.9 MPa
10000 psi
ASTM D790
Flexural Modulus 2.52 GPa
365 ksi
Method I (3 point load), Procedure B); ASTM D790
Izod Impact, Notched 1.43 J/cm
2.67 ft-lb/in
73°F; ASTM D256
Gardner Impact 10.17 J
7.500 ft-lb
ASTM D3029