Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Multibase SILASTIC® C7-4535 CADOX BSD Dow-Corning Biomedical Grade ETR Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Silicone, Thermoplastic
Manufacturer Multibase
Trade Name SILASTIC®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase SILASTIC® C7-4535 CADOX BSD Dow-Corning Biomedical Grade ETR Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Multibase
Mechanical Properties Metric English Comments
Hardness, Shore A 34
34
as molded
38
38
post cured- 2 hours at 177°C
41
41
post cured- 4 hours at 204°C
Tensile Strength, Ultimate 6.27 MPa
910 psi
post cured- 4 hours at 204°C
8.48 MPa
1230 psi
post cured- 2 hours at 177°C
8.96 MPa
1300 psi
as molded
Tensile Strength, Yield 1.31 MPa
190 psi
at 200%, as molded
1.45 MPa
210 psi
at 200%, post cured- 2 hours at 177°C
1.63 MPa
237 psi
200%, post cured- 4 hours at 204°C
Elongation at Break 643 %
643 %
post cured- 4 hours at 204°C
768 %
768 %
as molded
808 %
808 %
post cured- 2 hours at 177°C
Tear Strength 18.9 kN/m
108 pli
as molded; Die B
21.4 kN/m
122 pli
post cured- 2 hours at 177°C; Die B
23.3 kN/m
133 pli
post cured- 4 hours at 204°C; Die B