Multibase SILASTIC® C7-4535 CADOX TS-50S Dow-Corning Biomedical Grade ETR Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Silicone, Thermoplastic
Manufacturer Multibase
Trade Name SILASTIC®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase SILASTIC® C7-4535 CADOX TS-50S Dow-Corning Biomedical Grade ETR Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Multibase
Mechanical Properties Metric English Comments
Hardness, Shore A 29
29
as molded
32
32
post cured- 2 hours at 177°C
35
35
post cured- 4 hours at 204°C
Tensile Strength, Ultimate 5.14 MPa
745 psi
post cured- 4 hours at 204°C
8.20 MPa
1190 psi
post cured- 2 hours at 177°C
8.363 MPa
1213 psi
as molded
Tensile Strength, Yield 0.931 MPa
135 psi
at 200%, as molded
0.965 MPa
140 psi
at 200%, post cured- 2 hours at 177°C
1.28 MPa
185 psi
200%, post cured- 4 hours at 204°C
Elongation at Break 656 %
656 %
post cured- 4 hours at 204°C
971 %
971 %
post cured- 2 hours at 177°C
1015 %
1015 %
as molded
Tear Strength 22.4 kN/m
128 pli
as molded; Die B
24.5 kN/m
140 pli
post cured- 2 hours at 177°C; Die B
28.7 kN/m
164 pli
post cured- 4 hours at 204°C; Die B