Multibase SILASTIC® C7-4535 VAROX Dow-Corning Biomedical Grade ETR Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Silicone, Thermoplastic
Manufacturer Multibase
Trade Name SILASTIC®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase SILASTIC® C7-4535 VAROX Dow-Corning Biomedical Grade ETR Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Multibase
Mechanical Properties Metric English Comments
Hardness, Shore A 35
35
as molded
37
37
post cured- 2 hours at 177°C
40
40
post cured- 4 hours at 204°C
Tensile Strength, Ultimate 7.412 MPa
1075 psi
post cured- 4 hours at 204°C
8.115 MPa
1177 psi
as molded
10.12 MPa
1468 psi
post cured- 2 hours at 177°C
Tensile Strength, Yield 1.45 MPa
210 psi
at 200%, as molded
1.48 MPa
215 psi
at 200%, post cured- 2 hours at 177°C
1.59 MPa
230 psi
200%, post cured- 4 hours at 204°C
Elongation at Break 758 %
758 %
post cured- 4 hours at 204°C
912 %
912 %
as molded
1041 %
1041 %
post cured- 2 hours at 177°C
Tear Strength 26.8 kN/m
153 pli
as molded; Die B
27.3 kN/m
156 pli
post cured- 2 hours at 177°C; Die B
31.4 kN/m
179 pli
post cured- 4 hours at 204°C; Die B
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved