Multibase TPSiV™ 3010-50A Thermoplastic Silicone Vulcanizate

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Vulcanizate Elastomer (TPV) , Polyurethane, TP , Silicone, Thermoplastic
Manufacturer Multibase
Trade Name TPSiV™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase TPSiV™ 3010-50A Thermoplastic Silicone Vulcanizate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
These materials are a novel family of TPV products based on cross-linked silicone rubber dispersed into various engineering thermoplastics. The dispersion of the silicone internal phase is produced by dynamic “vulcanization” or cross-linking of silicone polymers within the thermoplastic organic phase and results in a stable droplet type morphology as shown in the TEM micrograph. TPSiV™ combines the elastomeric performance of silicone rubber with the melt re-processability and thermal and chemical resistance of engineering thermoplastics.Thermoplastic polyurethane based TPSiV™ (3010, 3011, 3111, 3040, 3340 grades) combine the benefits of excellent abrasion resistance from the polyurethane as well as the lower coefficient of friction and improved temperature properties from the silicone rubber.PSiV™ 3010-50A / 60A: Designed to have a low compression set and tension set as well as excellent dielectric strength. Recommended for injection molding applications and bonds to PC, ABS, PU, and PVC. The 60A product is plasticizer free.Information provided by Multibase, a Dow Corning Company
Physical Properties Metric English Comments
Specific Gravity 1.12 g/cc
1.12 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 52
52
10 sec; ASTM D2240
Tensile Strength at Break 7.10 MPa
1030 psi
ASTM D412
Elongation at Break 470 %
470 %
ASTM D412
Tear Strength 24.5 kN/m
140 pli
ASTM D412
Taber Abrasion, mg/1000 Cycles 21
21
ASTM D1044
Compression Set 14 %

@Temperature 22.8 °C,
Time 79200 sec
14 %

@Temperature 73.0 °F,
Time 22.0 hour
ASTM D412
49 %

@Temperature 70.0 °C,
Time 79200 sec
49 %

@Temperature 158 °F,
Time 22.0 hour
ASTM D412
74 %

@Temperature 120 °C,
Time 79200 sec
74 %

@Temperature 248 °F,
Time 22.0 hour
ASTM D412
Tensile Set 6.0 %
6.0 %
1; ASTM D412
20 %
20 %
3; ASTM D412
24 %
24 %
At Break; ASTM D412
24 %
24 %
ASTM D412
Electrical Properties Metric English Comments
Dielectric Constant 4.37
4.37
Dielectric Strength 19.0 kV/mm
483 kV/in
19.0 kV/mm

@Frequency 100 Hz
483 kV/in

@Frequency 100 Hz
Processing Properties Metric English Comments
Rear Barrel Temperature 180 °C
356 °F
Middle Barrel Temperature 190 °C
374 °F
Front Barrel Temperature 200 °C
392 °F
Nozzle Temperature 205 °C
401 °F
Mold Temperature 10.0 - 30.0 °C
50.0 - 86.0 °F
Drying Temperature 80.0 °C
176 °F
Dry Time 2 - 4 hour
2 - 4 hour
Descriptive Properties Value Comments
Injection Rate Fast