Murtfeldt Murinyl® Polyvinylidinefluoride

Category Polymer , Thermoplastic , Fluoropolymer , PVDF , Polyvinylidinefluoride (PVDF), Molded/Extruded
Manufacturer Murtfeldt Kunststoffe GmbH & Co
Trade Name Murinyl®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Murtfeldt Murinyl® Polyvinylidinefluoride.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
As a fluorinated plastic, Murinyl® is exceptionally resistant to chemicals, hydrolysis, and sterilization. Its properties change very little at high service temperatures and after long-term exposure to UV radiation. This material is ideally suited for use in the food sector and medical industry.Special Properties:• Good wear resistance• Good rigidity• High compressive strength• High constant service temperature• Good resistance to chemicals• Resistant to sterilization• No stress corrosion possible• Very good resistance to UV rays and adverse weather conditions• No moisture absorption• Approved for use in the food industry (EU and FDA)Information provided by Murtfeldt Kunststoffe GmbH & Co. KG.
Physical Properties Metric English Comments
Density 1.79 g/cc
0.0647 lb/in³
ISO 1183-1
Moisture Absorption at Equilibrium 0.010 %

@Temperature 23.0 °C
0.010 %

@Temperature 73.4 °F
50% RH
Water Absorption at Saturation 0.050 %

@Temperature 23.0 °C
0.050 %

@Temperature 73.4 °F
Mechanical Properties Metric English Comments
Hardness, Shore D 78
78
DIN 53505
Tensile Strength, Yield 50.0 MPa
7250 psi
ISO 527-1/-2
Creep Strength 10.0 MPa
1450 psi
stress leading to 1% elongation; ISO 899-1
Modulus of Elasticity 2.30 GPa
334 ksi
Compressive Yield Strength 17.0 MPa

@Strain 1.00 %
2470 psi

@Strain 1.00 %
dry; ISO 604
32.0 MPa

@Strain 2.00 %
4640 psi

@Strain 2.00 %
dry; ISO 604
Charpy Impact Unnotched NB
NB
ISO 179
Charpy Impact, Notched 1.00 J/cm²
4.76 ft-lb/in²
ISO 179-1/1eA
Coefficient of Friction, Dynamic 0.35
0.35
Sand Slurry 21
21
µm/km
Thermal Properties Metric English Comments
CTE, linear 125 µm/m-°C

@Temperature 23.0 - 60.0 °C
69.4 µin/in-°F

@Temperature 73.4 - 140 °F
140 µm/m-°C

@Temperature 23.0 - 100 °C
77.8 µin/in-°F

@Temperature 73.4 - 212 °F
Melting Point 175 °C
347 °F
ISO 11357-1
Maximum Service Temperature, Air 150 °C

@Time 7.20e+7 sec
302 °F

@Time 20000 hour
160 °C

@Time <=86400 sec
320 °F

@Time <=24.0 hour
Minimum Service Temperature, Air -50.0 °C
-58.0 °F
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
IEC 60093
Surface Resistance 1.00e+13 ohm
1.00e+13 ohm
IEC 60093
Dielectric Constant 6.0

@Frequency 1.00e+6 Hz
6.0

@Frequency 1.00e+6 Hz
IEC 60250
7.4

@Frequency 100 Hz
7.4

@Frequency 100 Hz
IEC 60250
Dielectric Strength 18.0 kV/mm
457 kV/in
IEC 60243-1
Dielectric Loss Index 0.025

@Frequency 100 Hz
0.025

@Frequency 100 Hz
IEC 60250
0.165

@Frequency 1.00e+6 Hz
0.165

@Frequency 1.00e+6 Hz
IEC 60250
Compliance Properties Metric English Comments
FDA Yes
Yes
Descriptive Properties Value Comments
Color Natural