Material Notes:
Murylon® B natural has the best impact resistance of all Murylon materials. This material is especially suited for use in machine construction thanks to an excellent combination of mechanical properties.Special Properties:• Exceptional resistance• Good impact strength• Low cold flow characteristics• Approved for use in the food industry (EU and FDAInformation provided by Murtfeldt Kunststoffe GmbH & Co. KG.
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
ISO 1183-1
Moisture Absorption at Equilibrium 2.6 %

@Temperature 23.0 °C
2.6 %

@Temperature 73.4 °F
50% RH
Water Absorption at Saturation 9.0 %

@Temperature 23.0 °C
9.0 %

@Temperature 73.4 °F
Mechanical Properties Metric English Comments
Hardness, Rockwell M 85
85
dry; ISO 2039-2
Hardness, Shore D 76
76
DIN 53505
Ball Indentation Hardness 150 MPa
21800 psi
dry; ISO 2039-1
Tensile Strength, Yield 45.0 MPa
6530 psi
50% RH; ISO 527-1
80.0 MPa
11600 psi
dry; ISO 527-1
Elongation at Break >= 50 %
>= 50 %
dry; ISO 527-1
>= 100 %
>= 100 %
50% RH; ISO 527-1
Creep Strength 7.00 MPa

@Time 3.60e+6 sec
1020 psi

@Time 1000 hour
stress leading to 1% elongation; 50% RH; ISO 899-1
18.0 MPa

@Time 3.60e+6 sec
2610 psi

@Time 1000 hour
stress leading to 1% elongation; dry; ISO 899-1
Modulus of Elasticity 1.425 GPa
206.7 ksi
50% RH
3.30 GPa
479 ksi
dry
Compressive Yield Strength 24.0 MPa

@Strain 1.00 %
3480 psi

@Strain 1.00 %
dry; ISO 604
46.0 MPa

@Strain 2.00 %
6670 psi

@Strain 2.00 %
dry; ISO 604
80.0 MPa

@Strain 5.00 %
11600 psi

@Strain 5.00 %
dry; ISO 604
Charpy Impact Unnotched NB
NB
dry; ISO 179-1/1eU
NB
NB
ISO 179
Charpy Impact, Notched 0.550 J/cm²
2.62 ft-lb/in²
dry; ISO 179-1/1eA
Coefficient of Friction, Dynamic 0.35
0.35
Sand Slurry 0.23
0.23
µm/km
Thermal Properties Metric English Comments
CTE, linear 90.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
50.0 µin/in-°F

@Temperature 73.4 - 140 °F
105 µm/m-°C

@Temperature 23.0 - 100 °C
58.3 µin/in-°F

@Temperature 73.4 - 212 °F
Thermal Conductivity 0.280 W/m-K
1.94 BTU-in/hr-ft²-°F
Melting Point 220 °C
428 °F
ISO 11357-1
Maximum Service Temperature, Air 70.0 °C

@Time 7.20e+7 sec
158 °F

@Time 20000 hour
85.0 °C

@Time 1.80e+7 sec
185 °F

@Time 5000 hour
160 °C

@Time <=86400 sec
320 °F

@Time <=24.0 hour
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Glass Transition Temp, Tg 50.0 °C
122 °F
ISO 11357-1
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Electrical Resistivity >= 1.00e+12 ohm-cm
>= 1.00e+12 ohm-cm
50% RH; IEC 60093
>= 1.00e+14 ohm-cm
>= 1.00e+14 ohm-cm
dry; IEC 60093
Surface Resistance >= 1.00e+12 ohm
>= 1.00e+12 ohm
50% RH; IEC 60093
>= 1.00e+13 ohm
>= 1.00e+13 ohm
dry; IEC 60093
Dielectric Constant 3.3

@Frequency 1.00e+6 Hz
3.3

@Frequency 1.00e+6 Hz
dry; IEC 60250
3.8

@Frequency 1.00e+6 Hz
3.8

@Frequency 1.00e+6 Hz
50% RH; IEC 60250
3.9

@Frequency 100 Hz
3.9

@Frequency 100 Hz
dry; IEC 60250
7.4

@Frequency 100 Hz
7.4

@Frequency 100 Hz
50% RH; IEC 60250
Dielectric Strength 16.0 kV/mm
406 kV/in
50% RH; IEC 60243-1
25.0 kV/mm
635 kV/in
dry; IEC 60243-1
Dielectric Loss Index 0.019

@Frequency 100 Hz
0.019

@Frequency 100 Hz
dry; IEC 60250
0.021

@Frequency 1.00e+6 Hz
0.021

@Frequency 1.00e+6 Hz
dry; IEC 60250
0.060

@Frequency 1.00e+6 Hz
0.060

@Frequency 1.00e+6 Hz
50% RH; IEC 60250
0.13

@Frequency 100 Hz
0.13

@Frequency 100 Hz
50% RH; IEC 60250
Compliance Properties Metric English Comments
European Food 1935/2004 Yes
Yes
FDA Yes
Yes
Descriptive Properties Value Comments
Color Natural/Black