Murtfeldt Original Material ”S”® plus + LF ESD Polyethylene, Low Friction Conductive

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), UHMW PE Ultra High Molecular Weight
Manufacturer Murtfeldt Kunststoffe GmbH & Co
Trade Name Original Material ”S”®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Murtfeldt Original Material ”S”® plus + LF ESD Polyethylene, Low Friction Conductive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This material is electrically conductive and has half the sliding friction coefficient of the Original Material ”S”® enabling voltage to be dissipated at maximum speed with the same maximum friction resistance.Special Properties: Extremely high conductivity Voltage dissipation on the surface in less than 0.1s Reduction in drive power with no reduction in performance Minimal and constant sliding friction coefficient even in continuous operation Self-lubricating Approved for use in the food industry (EU and/or FDA)Information provided by Murtfeldt Kunststoffe GmbH & Co. KG.
Physical Properties Metric English Comments
Density <= 0.930 g/cc
<= 0.0336 lb/in³
ISO 1183
Molecular Weight 9.00e+6 g/mol
9.00e+6 g/mol
Mechanical Properties Metric English Comments
Hardness, Shore D 60
60
DIN 53505
Ball Indentation Hardness 30.0 MPa
4350 psi
Tensile Strength 20.0 MPa
2900 psi
ISO 527
Elongation at Break 255 %
255 %
ISO 527
Modulus of Elasticity 0.700 GPa
102 ksi
Charpy Impact, Notched >= 15.0 J/cm²
>= 71.4 ft-lb/in²
ISO 179
Coefficient of Friction, Dynamic 0.060 - 0.10
0.060 - 0.10
Sand Slurry 80
80
value in %
Thermal Properties Metric English Comments
CTE, linear 200 µm/m-°C

@Temperature 23.0 - 60.0 °C
111 µin/in-°F

@Temperature 73.4 - 140 °F
Thermal Conductivity 0.400 W/m-K
2.78 BTU-in/hr-ft²-°F
ISO 52612
Maximum Service Temperature, Air 90.0 °C
194 °F
Short Term
80.0 °C

@Time 1.80e+7 sec
176 °F

@Time 5000 hour
Minimum Service Temperature, Air -200 °C
-328 °F
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Electrical Resistivity <= 1000 ohm-cm
<= 1000 ohm-cm
IEC 60093
Surface Resistance <= 1.00e+9 ohm
<= 1.00e+9 ohm
IEC 60093
Compliance Properties Metric English Comments
European Food 1935/2004 Yes
Yes
FDA Yes
Yes
Descriptive Properties Value Comments
Color Black