Mykroy/Mycalex MM 500 Machining Grade Glass-bonded Mica Composite

Category Ceramic , Glass , Glass Ceramic , Machinable Ceramic
Manufacturer Mykroy/Mycalex, Crystex Composites
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Mykroy/Mycalex MM 500 Machining Grade Glass-bonded Mica Composite.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Synthetic mica filler. Does not burn. Better radiation resistance (3 x 10^10 Rads-Cobalt) than grade 400.This ceramoplastic material is a versatile and efficient insulating material designed to meet the exacting demands of technical markets, worldwide. Glass-Bonded Mica is the only inorganic material to bridge the performance materials gap between organic plastics and ceramics.This unique high performance technical ceramic is a union of finely powered electrical quality glass and precisely defined and classified mica. The union of mica and glass takes place under simultaneous pressure and heat, transforming the materials into a new composition that inherits all the insulating advantages of both constituents.These materials are easily machined, mold like plastic, and have a wide range of operating temperatures. They find applications in the aircraft, laser, communications, aerospace, cryogenic, electronic, radiation, semiconductor, computer, automotive, and power distribution industries.Typical data below provided by Mykroy/Mycalex Ceramics.
Physical Properties Metric English Comments
Density 2.70 g/cc
0.0975 lb/in³
Moisture Absorption at Equilibrium 0.00 %
0.00 %
Nil
Mechanical Properties Metric English Comments
Hardness, Rockwell A 46
46
Hardness, Rockwell H 90
90
Tensile Strength, Ultimate 41.4 MPa
6000 psi
Modulus of Elasticity 82.7 GPa
12000 ksi
Flexural Strength 86.2 MPa
12500 psi
Compressive Strength 276 MPa
40000 psi
Izod Impact, Notched 0.908 J/cm
1.70 ft-lb/in
Thermal Properties Metric English Comments
CTE, linear 10.53 µm/m-°C

@Temperature 350 °C
5.850 µin/in-°F

@Temperature 662 °F
11.57 µm/m-°C

@Temperature 25.0 °C
6.428 µin/in-°F

@Temperature 77.0 °F
Specific Heat Capacity 0.5021 J/g-°C
0.1200 BTU/lb-°F
Thermal Conductivity 1.15 W/m-K
7.98 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 400 °C
752 °F
Continuous
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
Surface Resistivity per Square 1.00e+12 ohm
1.00e+12 ohm
Dielectric Constant 6.9

@Frequency 1e+6 Hz
6.9

@Frequency 1e+6 Hz
Dielectric Strength 20.9 kV/mm
530 kV/in
Dissipation Factor 0.0013

@Frequency 1e+6 Hz
0.0013

@Frequency 1e+6 Hz
Dielectric Loss Index 0.0090
0.0090
1 MHz
Arc Resistance 260 sec
260 sec
Descriptive Properties Value Comments
Color Light Gray