Material Notes:
Description: 1391 is a non-filled compounded polypropylene produced for automotive applications.Key Applications: Automotive exteriorInformation provided by Mytex Polymers
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D792
Melt Flow 28 g/10 min
28 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 71
71
ASTM D785
Tensile Strength, Yield 24.0 MPa
3480 psi
50 mm/min; ASTM D638
Flexural Modulus 1.25 GPa
181 ksi
Tangent; 1.3 mm/min; ASTM D790
Izod Impact, Notched 1.50 J/cm

@Temperature 23.0 °C
2.81 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 97.0 °C
207 °F
ASTM D648