Mytex Polymers AS33LW Polypropylene, Rubber modified, Talc filled, Compounded

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 10% Talc Filler
Manufacturer Mytex Polymers
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Mytex Polymers AS33LW Polypropylene, Rubber modified, Talc filled, Compounded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: AS33LW is a compounded, talc, rubber modified polypropylene for exterior automotive applications. Material has outstanding moldability and excellent balance of high stiffness and good impact performance properties.Key Applications: Automotive exterior, painted or mold-in-colorInformation provided by Mytex Polymers
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ASTM D792
Melt Flow 35 g/10 min
35 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 58
58
ASTM D785
Tensile Strength, Yield 21.0 MPa
3050 psi
50 mm/min; ASTM D638
Flexural Modulus 1.47 GPa
213 ksi
Tangent; 1.3 mm/min; ASTM D790
Izod Impact, Notched 6.00 J/cm

@Temperature 23.0 °C
11.2 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 95.0 °C
203 °F
ASTM D648