Material Notes:
Applications: Construction MaterialInformation provided by Nano Composite Materials Technology Limited
Physical Properties Metric English Comments
Density 1.11 g/cc
0.0401 lb/in³
NCMT Method
Melt Flow 24 g/10 min

@Load 2.16 kg,
Temperature 230 °C
24 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 40.0 MPa
5800 psi
ASTM D638
Elongation at Break 4.0 %
4.0 %
ASTM D638
Tensile Modulus 5.20 GPa
754 ksi
ASTM D638
Izod Impact, Notched 0.350 J/cm
0.656 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 160 °C
320 °F
Deflection Temp.; ASTM D648