ND Industries StudGrade® 131 Permanent CT Threadlocker

Category Polymer , Adhesive , Thermoset
Manufacturer ND Industries, Inc
Trade Name StudGrade®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ND Industries StudGrade® 131 Permanent CT Threadlocker.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
General DescriptionHigh strength threadlockers for maximum security. Suitable for most applications where disassembly is not required.Typical Usesstuds and bolts, and threaded pipe fittings.Meets military spec MIL-S-46163 Type II Grade O
Physical Properties Metric English Comments
Viscosity 1600 - 3000 cP
1600 - 3000 cP
Thixotropic
Mechanical Properties Metric English Comments
Impact Test 5.65 - 16.9 J
4.17 - 12.5 ft-lb
Prevail
16.9 - 28.2 J
12.5 - 20.8 ft-lb
Break
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 149 °C
300 °F
Minimum Service Temperature, Air -53.9 °C
-65.0 °F
Processing Properties Metric English Comments
Cure Time 5.00 min
0.0833 hour
With Primer (Fixture)
30.0 min
0.500 hour
On steel (fixture)
1440 min
24.0 hour
With Primer (Full)
1440 min
24.0 hour
On steel (Full)
Descriptive Properties Value Comments
Color Red
Gap Fill, in. 0.005