NEXA® PFX9020 Perfluoroelastomer

Category Polymer , Thermoset , Fluoropolymer, TS , Thermoset Fluoroelastomer , Rubber or Thermoset Elastomer (TSE)
Manufacturer NEXA® S.p.A.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NEXA® PFX9020 Perfluoroelastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
NEXA produces sealing elements for extreme and critical applications, particularly where high temperature, wet conditions (steam/water), purity and chemical resistance are important factors to consider. Applications include Aerospace, Automotive, Chemical, Food, Industrial, Pharmaceutical, Semiconductor, Nuclear, and Oil & Gas.
Mechanical Properties Metric English Comments
Hardness, Shore A 75 - 85

@Thickness 6.00 mm
75 - 85

@Thickness 0.236 in
DIN 53505
Tensile Strength >= 17.0 MPa
>= 2470 psi
DIN 53504
Elongation at Break >= 220 %
>= 220 %
DIN 53504
100% Modulus >= 0.00400 GPa
>= 0.580 ksi
DIN 53504
Compression Set <= 35 %

@Temperature 200 °C,
Time 259000 sec
<= 35 %

@Temperature 392 °F,
Time 72.0 hour
DIN 53517
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 300 °C
572 °F
Descriptive Properties Value Comments
Color Translucent