Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

NHEP Spectron™ E6046 Nylon 6, 15% Glass Fiber

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 20% Glass Fiber Filled
Manufacturer Ngai Hing Hong Engineering Plastic (Hong Kong) Ltd .
Trade Name Spectron™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NHEP Spectron™ E6046 Nylon 6, 15% Glass Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Natural color. E6046 exhibits high rigidity and mechanical strength. It is suitable for wide range of applications. Property data measured at room temperature, 50% RH.Information provided by Bieglo Gmbh for Ngai Hing Engineering Plastic (Hong Kong) Ltd.
Physical Properties Metric English Comments
Density 1.24 g/cc
0.0448 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0070 - 0.016 cm/cm
0.0070 - 0.016 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength 100 MPa
14500 psi
ASTM D638
Elongation at Yield 8.0 %
8.0 %
ASTM D638
Flexural Strength 150 MPa
21800 psi
ASTM D790
Flexural Modulus 4.30 GPa
624 ksi
ASTM D790
Izod Impact, Notched 1.00 J/cm
1.87 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Flammability, UL94 HB

@Thickness 3.17 mm
HB

@Thickness 0.125 in
Processing Properties Metric English Comments
Rear Barrel Temperature 220 - 230 °C
428 - 446 °F
Middle Barrel Temperature 230 - 240 °C
446 - 464 °F
Front Barrel Temperature 240 - 250 °C
464 - 482 °F
Nozzle Temperature 250 - 260 °C
482 - 500 °F
Drying Temperature 100 - 120 °C

@Time 7200 - 14400 sec
212 - 248 °F

@Time 2.00 - 4.00 hour
Descriptive Properties Value Comments
Processing Injection Pressure Medium-High
Processing Injection Speed Medium-High
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved