Category Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Molded, Unreinforced
Manufacturer NIZHNEKAMSKNEFTEKHIM Inc
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NIZHNEKAMSKNEFTEKHIM 585 General Purpose Polystyrene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Grade 585 is a high molecular weight, low melt-flow crystal polystyrene. This polymer is tailored for extruded foam applications such as egg cartons, meat trays and food service. It is also suited for production of oriented polystyrene sheet.Information provided by manufacturer
Physical Properties Metric English Comments
Melt Flow 1.5 - 3.5 g/10 min

@Load 5.00 kg,
Temperature 200 °C
1.5 - 3.5 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break >= 38.0 MPa
>= 5510 psi
ASTM D638
Flexural Strength >= 95.0 MPa
>= 13800 psi
ASTM D790
Thermal Properties Metric English Comments
Vicat Softening Point >= 98.0 °C
>= 208 °F
ASTM D1525
Chemical Properties Metric English Comments
Styrene Content <= 0.050 %
<= 0.050 %
p. 4.10 of the TU