Material Notes:
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Physical Properties Metric English Comments
Density 0.916 - 0.920 g/cc
0.0331 - 0.0332 lb/in³
Base Resin; ASTM D1505
Melt Flow 1.8 - 2.2 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.8 - 2.2 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1283/L
54 - 66 g/10 min

@Load 21.6 kg,
Temperature 190 °C
54 - 66 g/10 min

@Load 47.6 lb,
Temperature 374 °F
Flow@21.6kg/Flow@2.16kg ratio < 30; ASTM D1283
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD >= 51.0 MPa
>= 7400 psi
ASTM D882
Film Tensile Strength at Yield, TD >= 24.0 MPa
>= 3480 psi
ASTM D882
Film Elongation at Break, MD >= 500 %
>= 500 %
ASTM D882
Film Elongation at Break, TD >= 800 %
>= 800 %
ASTM D882
Tensile Modulus >= 0.130 GPa
>= 18.9 ksi
2% sec, MD; ASTM D882
>= 0.140 GPa
>= 20.3 ksi
2% sec, TD; ASTM D882
Elmendorf Tear Strength, MD >= 4.33 g/micron
>= 110 g/mil
ASTM D1922
Elmendorf Tear Strength, TD >= 14.6 g/micron
>= 370 g/mil
ASTM 1922
Dart Drop Test >= 80.0 g
>= 0.176 lb
ASTM D1709
Descriptive Properties Value Comments
Gel Content (pcs./m²) 0
> 1mm
245
(0.2-0.5)mm
250
> 0.2mm (totally)
5
(0.5-1.0)mm
Copyright © lookpolymers.com All Rights Reserved