Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

NOVA Chemicals Novapol® HB-L354-A HDPE Blow Molding Resin

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Blow Molding Grade
Manufacturer NOVA Chemicals
Trade Name Novapol®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NOVA Chemicals Novapol® HB-L354-A HDPE Blow Molding Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Good balance of physical and molding properties-high toughness, Excellent processability on high-speed, multiple-head blow molding lines, UL-94HB listedApplications: Household chemical bottles, Industrial chemical bottles, Automotive fluid bottles, ToysAdditives: Process stabilizerInformation provided by NOVA Chemicals.
Physical Properties Metric English Comments
Density 0.955 g/cc
0.0345 lb/in³
ASTM D792
Environmental Stress Crack Resistance 48 hour
48 hour
F<sub>50</sub>; Condition B, 100% Igepal; ASTM D1693
Melt Flow 0.30 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.30 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 31.0 MPa
4500 psi
50 mm/min; ASTM D638
Elongation at Break 900 %
900 %
50 mm/min; ASTM D638
Flexural Modulus 1.18 GPa
171 ksi
at 1% Secant; ASTM D790
Izod Impact, Notched 2.70 J/cm
5.06 ft-lb/in
ASTM D256
Processing Properties Metric English Comments
Melt Temperature 160 - 205 °C
320 - 401 °F