Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

NOVA Chemicals Novapol® HB-W555-EC HDPE Blow Molding Resin

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Blow Molding Grade
Manufacturer NOVA Chemicals
Trade Name Novapol®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NOVA Chemicals Novapol® HB-W555-EC HDPE Blow Molding Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
HB-W555-EC complies with the U.S. FDA specifications for olefin polymers and may be used in the U.S. as an article or component of an article intended for use in contact with food. It is also biologically and chemically inert.This resin can be blow molded on most commercial blow molding machines.Features: Low particle counts, Low leaching, Excellent long term container storage performance, High rigidity, Excellent impact strength, Excellent ESCRAdditives: Process StabilizerApplications: High purity chemical packaging, High performance packaging for food and flavourings
Physical Properties Metric English Comments
Density 0.955 g/cc
0.0345 lb/in³
ASTM D 792
ESCR 100% Igepal® >= 500 hour
>= 500 hour
F50, Condition A; ASTM D 1693
High Load Melt Index 5.0 g/10 min

@Load 21.6 kg,
Temperature 190 °C
5.0 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ASTM D 1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 28.0 MPa
4060 psi
ASTM D 638
Elongation at Break 830 %
830 %
ASTM D 638
Flexural Modulus 1.40 GPa
203 ksi
ASTM D 790
Izod Impact, Unnotched 7.20 J/cm

@Thickness 3.20 mm
13.5 ft-lb/in

@Thickness 0.126 in
ASTM D 256
Tensile Impact Strength 420 kJ/m²
200 ft-lb/in²
ASTM D 1822
Thermal Properties Metric English Comments
Brittleness Temperature <= -100 °C
<= -148 °F
F50, notched specimen; ASTM D 746
Processing Properties Metric English Comments
Melt Temperature 180 - 220 °C
356 - 428 °F
Recommended
Copyright © lookpolymers.com All Rights Reserved