NOVA Chemicals Novapol® HP-Y353-A HDPE Pipe Coating Resin

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Pipe Grade
Manufacturer NOVA Chemicals
Trade Name Novapol®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NOVA Chemicals Novapol® HP-Y353-A HDPE Pipe Coating Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Good ESCR, Excellent toughness, High strength, Excellent processability, Excellent stiffnessApplications: For profile, corrugated non-pressure pipes, For storm and sanitary sewer pipe, For culvert and conduit applicationAdditives: Antioxidants and processing stabilizersInformation provided by NOVA Chemicals.
Physical Properties Metric English Comments
Density 0.9535 g/cc
0.03445 lb/in³
ASTM D792
ESCR 10% Igepal® >= 75 hour

@Temperature 50.0 °C
>= 75 hour

@Temperature 122 °F
F<sub>0-</sub>; ASTM D1693
Melt Flow 0.30 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.30 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 65
65
ASTM D2240
Tensile Strength, Yield 27.0 MPa
3920 psi
Extension rate 2 in/min; ASTM D638
Elongation at Break >= 900 %
>= 900 %
Extension rate 2 in/min; ASTM D638
Flexural Modulus 1.035 GPa
150.1 ksi
Secant 2% Strain; ASTM D3350
1.24 GPa
180 ksi
Tangent; ASTM D790
Thermal Properties Metric English Comments
CTE, linear 140 µm/m-°C

@Temperature 20.0 °C
77.8 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Melting Point 132 °C
270 °F
ASTM D3417
Maximum Service Temperature, Air 264 °C
507 °F
ASTM D3350
Vicat Softening Point 126 °C
259 °F
ASTM D1525
Brittleness Temperature <= -70.0 °C
<= -94.0 °F
F<sub>0</sub> notched specimen; ASTM D746
Processing Properties Metric English Comments
Melt Temperature 175 - 220 °C
347 - 428 °F