NOVA Chemicals Novapol® LF-0718-A-INJECTION LDPE Injection Molding Resin

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Molded
Manufacturer NOVA Chemicals
Trade Name Novapol®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NOVA Chemicals Novapol® LF-0718-A-INJECTION LDPE Injection Molding Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LF-0718-A complies with the U.S. FDA specifications for olefin polymers and may be used in the U.S. as an article or component of an article intended for use in contact with food. LF-0718-A is subject to the specific limitation that it may not be used in articles used for packing or holding food during cooking. This resin is biologically and chemically inert.Features: Excellent balance of toughness and softness, Good processability and dimensional stabilityApplications: Caps and closures, including tamper evident closures
Physical Properties Metric English Comments
Density 0.917 g/cc
0.0331 lb/in³
ASTM D 792
Melt Flow 7.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
7.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D 1238
Mechanical Properties Metric English Comments
Hardness, Shore D 53
53
ASTM D 2240
Tensile Strength at Break 11.0 MPa
1600 psi
ASTM D 638
Tensile Strength, Yield 9.00 MPa
1310 psi
ASTM D 638
Elongation at Break 548 %
548 %
ASTM D 638
Flexural Modulus 0.211 GPa
30.6 ksi
2% Secant; ASTM D 790
Flexural Modulus, 1% Secant 236 MPa
34200 psi
ASTM D 790
Thermal Properties Metric English Comments
Vicat Softening Point 83.0 °C
181 °F
ASTM D 1525