Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

NOVA Chemicals Sclair® 2315 LLDPE Injection Molding Resin  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE), Injection Molded
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NOVA Chemicals Sclair® 2315 LLDPE Injection Molding Resin  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: Low odor, low warpage, fast cycling, high surface gloss, permits light weight lid design, low temperature impact excellent.Data provided by the manufacturer.
Physical Properties Metric English Comments
Density 0.931 g/cc
0.0336 lb/in³
ASTM D792
Melt Flow 63 g/10 min

@Load 2.16 kg,
Temperature 190 °C
63 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 56
56
ASTM D2240
Tensile Strength, Yield 14.0 MPa
2030 psi
50 mm/min; ASTM D638
17.0 MPa
2470 psi
500 mm/min; ASTM D638
Flexural Modulus 0.520 GPa
75.4 ksi
ASTM D790
Thermal Properties Metric English Comments
Vicat Softening Point 100 °C
212 °F
ASTM D1525
Brittleness Temperature <= -60.0 °C
<= -76.0 °F
ASTM D696
Processing Properties Metric English Comments
Melt Temperature 170 - 260 °C
338 - 500 °F
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved