Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

NOVA Chemicals Sclair® 35BPM MDPE Extrusion Resin, 2.2% Carbon Black Filled  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , MDPE , Medium Density Polyethylene (MDPE), Extruded
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NOVA Chemicals Sclair® 35BPM MDPE Extrusion Resin, 2.2% Carbon Black Filled  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: Excellent ESCR, medium molecular weight, good processability, excellent long term thermal stability, good chemical resistance, excellent UV stability.Applications: Extrusion on to metal pipe to produce a corrosion resistant coating for buried pipe systems.Data provided by the manufacturer.
Physical Properties Metric English Comments
Density 0.939 g/cc
0.0339 lb/in³
Base Density
Water Absorption 0.010 %
0.010 %
ASTM D570
Environmental Stress Crack Resistance 1000 hour
1000 hour
Melt Flow 0.32 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.32 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 60
60
ASTM D2240
Tensile Strength, Ultimate 26.0 MPa
3770 psi
ASTM D638
Tensile Strength, Yield 18.0 MPa
2610 psi
ASTM D638
Elongation at Break 800 %
800 %
ASTM D638
Flexural Modulus 0.590 GPa
85.6 ksi
ASTM D790
Thermal Properties Metric English Comments
Melting Point 128 °C
262 °F
ASTM D3417
Vicat Softening Point 120 °C
248 °F
ASTM D1525
Brittleness Temperature <= -100 °C
<= -148 °F
ASTM D696