Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

NOVA Chemicals Sclair® 58G (High Gloss) HDPE Blow Molding Resin  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Blow Molding Grade
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NOVA Chemicals Sclair® 58G (High Gloss) HDPE Blow Molding Resin  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: Outstanding gloss, pearlescent finish when colored, good processability.Applications: Small part blow molding, injection blow molding, low-moderate ESCR uses.Data provided by the manufacturer.
Physical Properties Metric English Comments
Density 0.958 g/cc
0.0346 lb/in³
ASTM D792
Environmental Stress Crack Resistance 20 hour
20 hour
F50, Condition A, ASTM D1693, 100% Igepal
Melt Flow 0.96 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.96 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 67
67
ASTM D2240
Tensile Strength, Yield 28.0 MPa
4060 psi
ASTM D638
Elongation at Break 1200 %
1200 %
at 50 mm/min; ASTM D638
Flexural Modulus 1.10 GPa
160 ksi
ASTM D790
Thermal Properties Metric English Comments
Vicat Softening Point 126 °C
259 °F
ASTM D1525
Brittleness Temperature <= -70.0 °C
<= -94.0 °F
ASTM D696
Processing Properties Metric English Comments
Melt Temperature 170 - 215 °C
338 - 419 °F