NOVA Chemicals Styrocell® D933A Expandable Polystyrene  (discontinued **)

Category Polymer , Thermoplastic , Polystyrene (PS) , Expanded Polystyrene (EPS)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NOVA Chemicals Styrocell® D933A Expandable Polystyrene  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This grade is a special molding grade consisting of spherical polystyrene beads containing pentane as expansion agent, typically used for dry molding of drinking cups and thin wall containers.Applications: This grade is used for dry molding of drinking cups and containers with very thin walls such as vending cups.This grade complies with major European and US food contact regulatory regimes, including: European Community Directive 90/128/ECC, including 92/39EEC and 95/EC, relating to plastics materials and articles, intended to come into contact with foodstuffs. Dutch Food Packaging Regulations. Recommendations of German Federal Office of Health (BGA), now regulated by the new Institute of Consumer Health (BGVV), Empfehlung V. US Food and Drug Administration Code of Federal Regulations title 21, sections 177.1640 (Polystyrene) and 178.3010 (Blowing Agents).Information provided by NOVA Chemicals.
Physical Properties Metric English Comments
Bulk Density 0.620 g/cc
0.0224 lb/in³
Density >= 0.0300 g/cc
>= 0.00108 lb/in³
Minimum achievable; Single stage pre-expansion in continuous expander at atmospheric pressure
0.0700 - 0.100 g/cc
0.00253 - 0.00361 lb/in³
Normal molded density
Bead Size 0.200 - 0.350 mm
0.00787 - 0.0138 in
0.200 - 0.400 mm
0.00787 - 0.0157 in
Breda Laboratory Analytical Methods 90.30
Chemical Properties Metric English Comments
Styrene Content <= 0.10 %
<= 0.10 %
Residual Styrene Monomer Content per Breda Laboratory Analytical Methods 90.16
Blowing Agent Content >= 5.7 %
>= 5.7 %
Breda Laboratory Analytical Methods 90.18