NOVA Chemicals Surpass® IFs932-R Octene SLLDPE Injection Molding Resin

Category Polymer , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE), Injection Molded
Manufacturer NOVA Chemicals
Trade Name Surpass®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NOVA Chemicals Surpass® IFs932-R Octene SLLDPE Injection Molding Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
IFs932-R complies with the U.S. FDA regulations for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food.NOVA Chemicals' polyethylene resins are biologically and chemically inert.Features: Excellent balance of stiffness and toughness to meet application requirements, Low viscosity for exceptional processability yielding shorter cycle times and energy savings, Increases opportunities for light-weighting of lid designs, Low warpage for improved part quality and reliability, Superior organoleptic properties, Excellent contact clarity propertiesAdditives: Antioxidant, Mold releaseApplications: Lids, for non-frozen, thin wall, food packaging containers
Physical Properties Metric English Comments
Density 0.932 g/cc
0.0337 lb/in³
ASTM D 792
Melt Flow 150 g/10 min

@Load 2.16 kg,
Temperature 190 °C
150 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D 1238
Spiral Flow 50.8 cm
20.0 in
NOVA Chemicals snake flow number
Mechanical Properties Metric English Comments
Hardness, Shore D 60
60
ASTM D 2240
Tensile Strength at Break 10.0 MPa
1450 psi
Rate of 50 mm/min; ASTM D 638
Tensile Strength, Yield 16.0 MPa
2320 psi
Rate of 50 mm/min; ASTM D 638
Elongation at Break 35 %
35 %
Rate of 50 mm/min; ASTM D 638
Elongation at Yield 11 %
11 %
Rate of 50 mm/min; ASTM D 638
Tensile Modulus 0.700 GPa
102 ksi
1% Secant; ASTM D 638
Flexural Modulus, 1% Secant 580 MPa
84100 psi
ASTM D 790
Thermal Properties Metric English Comments
Vicat Softening Point 98.0 °C
208 °F
ASTM 1525