NYCOA 2263 Copolymer Nylon Alloy

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Unreinforced
Manufacturer NYCOA, Inc.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NYCOA 2263 Copolymer Nylon Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
monofilament weed eater, fishing lineInformation provided by NYCOA, Inc.
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
ISO 176
Mechanical Properties Metric English Comments
Tensile Strength, Yield 58.0 MPa
8410 psi
ISO METHOD 527
Elongation at Break >= 500 %
>= 500 %
ISO METHOD 527
Flexural Yield Strength 18.0 MPa
2610 psi
ISO METHOD 176
Flexural Modulus 0.345 GPa
50.0 ksi
ISO METHOD 178
Izod Impact, Notched 2.79 J/cm
5.23 ft-lb/in
ISO METHOD 180
Thermal Properties Metric English Comments
Melting Point 192 °C
378 °F
ISO METHOD 3146C
Processing Properties Metric English Comments
Processing Temperature 250 °C
482 °F
Rear Barrel Temperature 200 °C
392 °F
Middle Barrel Temperature 230 °C
446 °F
Front Barrel Temperature 250 °C
482 °F
Drying Temperature 76.0 °C
169 °F