NYCOA 5100 HS Heat Stabilized, Impact Modified Nylon 66 Resin

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Heat Stabilized
Manufacturer NYCOA, Inc.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NYCOA 5100 HS Heat Stabilized, Impact Modified Nylon 66 Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
NYCOA 5100 HS is an impact modified, heat stabilized Nylon 66 resin used for injection molding. This material is specially formulated to provide improved flexibility and ductility vs standard Nylon 66. NYCOA 5100 HS offers outstanding toughness, exceptional processability, and a greater service life at elevated temperatures than standard grades of Nylon 66. It is available in UV stable, and custom colors grades. It also has excellent chemical resistance to greases, oils, and other hydrocarbons. Typical applications include automotive wiring harnesses, motor component housings, gears, and electrical connectors.Information provided by Nycoa, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.12 g/cc
1.12 g/cc
ASTM D792
Water Absorption 1.2 %
1.2 %
24 hours; ASTM D570
Linear Mold Shrinkage 0.015 cm/cm
0.015 in/in
ASTM D955
Linear Mold Shrinkage, Transverse 0.016 cm/cm
0.016 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 118
118
ASTM D785
Tensile Strength, Yield 65.0 MPa
9430 psi
ASTM D638
Elongation at Break 50 %
50 %
ASTM D638
Flexural Strength 85.0 MPa
12300 psi
ASTM D790
Flexural Modulus 2.22 GPa
322 ksi
ASTM D790
Izod Impact, Notched 1.35 J/cm
2.53 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 258 °C
496 °F
ASTM D789
Deflection Temperature at 0.46 MPa (66 psi) 189 °C
372 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 70.0 °C
158 °F
ASTM D648