Material Notes:
The homogeneous phase constitution and very low amount of impurities offers considerable advantages over naturally occurring alumosilicates. The synthesized mullite product shows very good chemical uniformity, high refractory properties and excellent high temperature stability.
Physical Properties Metric English Comments
Bulk Density 2.80 g/cc
0.101 lb/in³
Density 3.13 g/cc
0.113 lb/in³
Water Absorption 0.50 %
0.50 %
Open Porosity 1.5 %
1.5 %
Component Elements Properties Metric English Comments
Al2O3 72 %
72 %
CaO+MgO 0.30 %
0.30 %
Fe2O3 0.30 %
0.30 %
Na2O or K2O 0.60 %
0.60 %
SiO2 26.5 %
26.5 %
TiO2 0.20 %
0.20 %
ZrO2 0.00 %
0.00 %
Descriptive Properties Value Comments
Baddeleyite % 0
Corundum % 1
Glassy Phase % 5.0-10.0
Mullite % 90-95