Material Notes:
NanoActive Al2O3 Plus is produced using proprietary processes to obtain high specific surface area, high porosity (75% are mesopores), low density, weakly aggregated material possessing high adsorption capacity and chemical reactivity.Applications: Applications include air cleaning, catalysts supports, coatings and binders, destruction of chemical warfare agents, heat transfer fluids (suspensions), polishing materials, polymer nanocomposites for improved tribological performance, smoke obscurant, and structural ceramics.Information provided by NanoScaleComposition based on metal
Physical Properties Metric English Comments
Bulk Density 0.200 g/cc
0.00723 lb/in³
Density 2.90 g/cc
0.105 lb/in³
Loss On Ignition <= 13 %
<= 13 %
Particle Size 5.0 µm
5.0 µm
mean aggregate size
Specific Surface Area >= 550 m²/g
>= 550 m²/g
BET
Pore Size 0.0110 microns
0.000433 mil
Average Diameter
Component Elements Properties Metric English Comments
Aluminum, Al >= 99.2 %
>= 99.2 %
Processing Properties Metric English Comments
Moisture Content <= 12 %
<= 12 %
Descriptive Properties Value Comments
Appearance / Color White Powder
Crystallite Size Amorphous
Minimum Total Pore Volume cc/g 1.5