Network Polymers NPP 50-0151

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Injection Molded
Manufacturer Network Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Network Polymers NPP 50-0151.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: High Density Polyethylene (HDPE)Information provided by Network Polymers Inc.
Physical Properties Metric English Comments
Density 0.951 g/cc
0.0344 lb/in³
ASTM D1505
High Load Melt Index 11.5 g/10 min

@Load 21.6 kg,
Temperature 190 °C
11.5 g/10 min

@Load 47.6 lb,
Temperature 374 °F
Procedure A Condition F (HLMI); ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 26.5 MPa
3840 psi
chs 2 in/min; ASTM D638
Elongation at Break >= 600 %
>= 600 %
chs 2 in/min; ASTM D638
Flexural Modulus 1.17 GPa
170 ksi
ASTM D790
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 73.0 °C
163 °F
ASTM D1525
Brittleness Temperature <= -76.1 °C
<= -105 °F
ASTM D746