Network Polymers Softflex® 0250

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber
Manufacturer Network Polymers
Trade Name Softflex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Network Polymers Softflex® 0250.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc.
Physical Properties Metric English Comments
Specific Gravity 0.890 g/cc
0.890 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.017 cm/cm

@Thickness 3.17 mm
0.017 in/in

@Thickness 0.125 in
ASTM D955
Linear Mold Shrinkage, Transverse 0.015 cm/cm

@Thickness 3.17 mm
0.015 in/in

@Thickness 0.125 in
ASTM D955
Melt Flow 0.20 g/10 min

@Load 2.16 kg,
Temperature 150 °C
0.20 g/10 min

@Load 4.76 lb,
Temperature 302 °F
Procedure A Condition C; ASTM D1238
52.7 g/10 min

@Load 2.16 kg,
Temperature 190 °C
52.7 g/10 min

@Load 4.76 lb,
Temperature 374 °F
Procedure A Condition E; ASTM D1238
110 g/10 min

@Load 1.00 kg,
Temperature 235 °C
110 g/10 min

@Load 2.20 lb,
Temperature 455 °F
Procedure A Condition Q; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 20 - 30
20 - 30
10 second dwell; ASTM D2240
24 - 34
24 - 34
Instantaneous; ASTM D2240
Tensile Strength, Yield 5.52 MPa
800 psi
chs 20 in/min; ASTM D412
Elongation at Break 950 %
950 %
ASTM D412
Gardner Impact >= 36.2 J

@Temperature -30.0 °C
>= 26.7 ft-lb

@Temperature -22.0 °F
ASTM D5420
Tear Strength 19.3 kN/m
110 pli
ASTM D624