Material Notes:
Blend, polyethylene, and FDA-approved active component. Non-toxic, non-abrasive, and safe. Ready to use and easy to remove.PURGEX 456 Plus is used for color and/or material changes and the removal of residual contamination in thermoplastic injection molding, extrusion, or blow molding equipment. PURGEX 456 Plus will efficiently purgehe barrel, screw, and nozzle, as well as hot runners. This blend removes all types of colorants and commodity resins, including polypropylene, polyethylene, and their copolymers. PURGEX 456 Plus is used to neutralize HCl gasses in PVC purging applications. PURGEX 456 Plus assures rapid turnaround on color and material changes with polyolefins and their copolymers, styrenics polymers, acetals, vinyls, TPO, TPU, and many more resins processed in this temperature range.
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 138 - 288 °C
280 - 550 °F