Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

NextGen Adhesives P907-12 Fiber Optic Adhesive

Category Polymer , Adhesive
Manufacturer NextGen Adhesives
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NextGen Adhesives P907-12 Fiber Optic Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: NGAC P907-12 is a rapid curing, low viscosity, heat cured epoxy adhesive system that is specifically formulated for use in the fiber optic industry.Advantages and Applications: Uses include bonding fiber optic bundles, potting glass fiber bundles and termination of single mode and multimode fiber optic connectors. NGAC P907-12 is a low viscosity mixture that ensures exceptional wicking and wetting of the fibers, along with superior adhesion strength. Additionally, it provides excellent thermal and moisture resistance.Information Provided by Nextgen Adhesives
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
Solids Content 100 %
100 %
Viscosity 2000 cP
2000 cP
Mechanical Properties Metric English Comments
Hardness, Shore D >= 85
>= 85
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 175 °C
347 °F
Minimum Service Temperature, Air -60.0 °C
-76.0 °F
Glass Transition Temp, Tg 115 °C
239 °F
Optical Properties Metric English Comments
Refractive Index 1.56
1.56
Processing Properties Metric English Comments
Cure Time 1.00 min

@Temperature 150 °C
0.0167 hour

@Temperature 302 °F
5.00 min

@Temperature 125 °C
0.0833 hour

@Temperature 257 °F
15.0 min

@Temperature 100 °C
0.250 hour

@Temperature 212 °F
Pot Life 60 - 120 min
60 - 120 min
Descriptive Properties Value Comments
Color Reddish Brown
Mix Ratio by Weight (R/H) 100/10
Users viewing this material also viewed the following: