Niche Polymer PPCG20BK Copolymer PP, 20% Glass Fiber Filled

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer , Polypropylene with 20% Glass Fiber Filler
Manufacturer Niche Polymer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Niche Polymer PPCG20BK Copolymer PP, 20% Glass Fiber Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Niche Polymer
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.00400 - 0.00700 cm/cm
0.00400 - 0.00700 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 60.7 MPa
8800 psi
ASTM D638
Elongation at Break 7.00 - 12.0 %
7.00 - 12.0 %
ASTM D638
Flexural Strength 73.1 MPa
10600 psi
ASTM D790
Flexural Modulus 3.31 GPa
480 ksi
ASTM D790
Izod Impact, Unnotched 0.908 J/cm

@Thickness 3.17 mm
1.70 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 138 °C
280 °F
ASTM D648
Processing Properties Metric English Comments
Melt Temperature 149 - 171 °C
300 - 340 °F
ASTM D789
Descriptive Properties Value Comments
Color Black