Niche Polymer PPCM6BK Copolymer PP

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Niche Polymer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Niche Polymer PPCM6BK Copolymer PP.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Niche Polymer
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.000150 - 0.000300 cm/cm
0.000150 - 0.000300 in/in
ASTM D955
Melt Flow 6.00 g/10 min

@Load 2.16 kg,
Temperature 230 °C
6.00 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D123
Mechanical Properties Metric English Comments
Tensile Strength at Break >= 24.1 MPa
>= 3500 psi
ASTM D638
Elongation at Break 300 %
300 %
ASTM D638
Flexural Strength 27.6 MPa
4000 psi
ASTM D790
Flexural Modulus >= 0.965 GPa
>= 140 ksi
ASTM D790
Izod Impact, Unnotched 1.07 J/cm

@Thickness 3.17 mm
2.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
Processing Properties Metric English Comments
Melt Temperature 149 - 171 °C
300 - 340 °F
ASTM D789
Descriptive Properties Value Comments
Color Black