Nitriflex SB-4022 Styrene Butadiene Copolymer

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Styrene Butadiene Rubber
Manufacturer Nitriflex
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Nitriflex SB-4022 Styrene Butadiene Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: Powdered rubber. Enables a lower mixing time and better homogenization, presenting a reduced generation of residues. Recommended for shoe soles, adhesives and seals, injected and molded artifacts. Information provided by Dax Resinas
Physical Properties Metric English Comments
Volatiles 0.00 - 0.75 %
0.00 - 0.75 %
Method B-003; ASTM D5668
Particle Size <= 1000 µm
<= 1000 µm
99-100%; ASTM D1921
Mooney Viscosity 46 - 58

@Temperature 100 °C
46 - 58

@Temperature 212 °F
MML1+4, Method B-002; ASTM D1646
Chemical Properties Metric English Comments
Styrene Content 22.5 - 24.5 %
22.5 - 24.5 %
ASTM D5775
Descriptive Properties Value Comments
CaCO3 Partitioning Agent Content % 10 to 14
Method B-035