Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

North Wood Plastics 60 HDPE + UNIFILL (40% Wood Fiber)

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Wood Filled
Manufacturer North Wood Plastics
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF North Wood Plastics 60 HDPE + UNIFILL (40% Wood Fiber).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by North Wood Plastics, Inc. UNIFILL-60 is a general purpose polyolefin compound compatible in both PP and HDPE. It is a masterbatch with 60% high quality pine wood flour filler. It is made with only the highest quality recycled resins. 1:2 HDPE:UNIFILL-60 yields an end product with 40% fiber.
Physical Properties Metric English Comments
Density 1.071 g/cc
0.03869 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0066 cm/cm
0.0066 in/in
ASTM D955
Melt Flow 0.70 g/10 min

@Temperature 190 °C
0.70 g/10 min

@Temperature 374 °F
Mechanical Properties Metric English Comments
Tensile Strength, Yield 15.0 MPa
2180 psi
ASTM D638
Elongation at Break 3.7 %
3.7 %
ASTM D638
Tensile Modulus 3.80 GPa
551 ksi
ASTM D638
Flexural Yield Strength 43.0 MPa
6240 psi
ASTM D790
Flexural Modulus 2.10 GPa
305 ksi
ASTM D790
Izod Impact, Notched 0.320 J/cm
0.599 ft-lb/in
ASTM D256
Izod Impact, Unnotched 0.910 J/cm
1.70 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 49.0 °C
120 °F
ASTM D648
Processing Properties Metric English Comments
Processing Temperature <= 200 °C
<= 392 °F
To prevent fiber degradation.
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved