Material Notes:
MCP-V40A is a polyurethane gel formulation specifically designed for padding and cushioning applications, where low rebound property of the material is critical. This viscoelastic polymer is a two-component urethane casting system, which can easily be processed to make variety of products in various vibration-dampening, shock absorbing, and cushioning applications. The impact absorption property can be indicated by rebound property of the material. The test data on standard polyurethane gel formulation MPP-V37A is there to show the enhanced low-rebound property of MCP-V40A. Polyurethane gel class polymers in general are made in such way that user can easily control the hardness of the product by simply changing the mixing ratio of the same combination of two component materials. This means MCP-V40A and other polyurethane gel systems can be used in a range of various applications, which require different hardness.Information provided by Northstar Polymers.
Processing Properties Metric English Comments
Processing Temperature 21.1 - 32.2 °C
70.0 - 90.0 °F
Prepolymer Temperature
21.1 - 32.2 °C
70.0 - 90.0 °F
Curing Agent Temperature
Mold Temperature 21.1 - 32.2 °C
70.0 - 90.0 °F
Cure Time 180 - 360 min

@Temperature 25.0 °C
3.00 - 6.00 hour

@Temperature 77.0 °F
De-mold Time
4320 - 7200 min

@Temperature 25.0 °C
72.0 - 120 hour

@Temperature 77.0 °F
Complete Cure Cycle
Pot Life 15.0 - 20.0 min
15.0 - 20.0 min
Descriptive Properties Value Comments
Curing Agent CPB-046
Prepolymer MPC-023
Weight Ratio 1:2.25
Prepolymer to Curing Agent Ratio