Material Notes:
Novacycle® 501 is a general purpose, rigid, extrusion grade PVC compound in pellet form. This formulation is designed to provide an economical alternative for extruded profiles Raw material appearance is Opaque Pellets. Applications: Novacycle® 501 is used for extruded profiles.Information supplied by the manufacturer.
Physical Properties Metric English Comments
Density 1.33 - 1.37 g/cc
0.0480 - 0.0495 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 36.5 - 44.1 MPa
5290 - 6400 psi
ASTM D638
Modulus of Elasticity 2.21 - 2.90 GPa
321 - 421 ksi
ASTM D638
Flexural Yield Strength 75.8 - 82.7 MPa
11000 - 12000 psi
ASTM D790
Flexural Modulus 2.07 - 2.90 GPa
300 - 421 ksi
ASTM D790
Izod Impact, Notched 1.07 - 7.47 J/cm
2.00 - 14.0 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 64.0 - 68.0 °C
147 - 154 °F
ASTM D648