Novatec Novaloy® 9000 PVC + ABS

Category Polymer , Thermoplastic , ABS Polymer , ABS/PVC Alloy , Vinyl (PVC)
Manufacturer Novatec
Trade Name Novaloy®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Novatec Novaloy® 9000 PVC + ABS.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Novaloy® 9000 is a specialty engineering alloy of ABS/PVC designed for injection molding, profile and sheet extrusion. Novaloy® 9000 has been formulated to provide excellent processing characteristics, high heat distortion temperatures along with excellent retention of physical properties upon aging. Impact resistance is excellent at both room and low temperature. Raw material appearance is Colored Opaque Pellets.Applications: Products made from Novaloy® 9000 are suitable for a variety of applications such as appliance housings, electrical boxes, communications, lawn and garden applications as well as recreational.Information supplied by the manufacturer.
Physical Properties Metric English Comments
Density 1.19 - 1.23 g/cc
0.0430 - 0.0444 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 42.2 MPa
6120 psi
ASTM D638
Modulus of Elasticity 2.41 GPa
350 ksi
ASTM D638
Flexural Yield Strength 75.2 MPa
10900 psi
ASTM D790
Flexural Modulus 2.41 GPa
350 ksi
ASTM D790
Izod Impact, Notched 4.00 J/cm
7.49 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 76.9 °C
170 °F
ASTM D648
Oxygen Index 31 %
31 %