Nyco NYAD® G Special Wollastonite

Category Ceramic , Oxide , Silicon Oxide , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Nyco
Trade Name NYAD®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Nyco NYAD® G Special Wollastonite.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Wollastonite (calcium metasilicate, or CaSiO3) is a naturally occurring white, non-metallic mineral with an acicular or needle-shaped crystal structure. This distinctive property makes wollastonite an ideal performance mineral for a broad range of industrial and consumer applications.Information provided by NYCO Minerals.
Physical Properties Metric English Comments
Specific Gravity 2.90 g/cc
2.90 g/cc
Bulk Density 0.368 g/cc
0.0133 lb/in³
loose
0.721 g/cc
0.0260 lb/in³
Tapped
Brightness 85 %
85 %
G.E. Brightness
Oil Absorption 47 %
47 %
Solubility of Water 0.0095 %
0.0095 %
Particle Size 45 µm
45 µm
D50
pH 9.9
9.9
10% Slurry
Molecular Weight 116 g/mol
116 g/mol
Mechanical Properties Metric English Comments
Hardness, Mohs 4.5
4.5
Thermal Properties Metric English Comments
CTE, linear 6.50 µm/m-°C

@Temperature 20.0 °C
3.61 µin/in-°F

@Temperature 68.0 °F
Melting Point 1410 °C
2570 °F
ASTM D1857
1540 °C
2800 °F
theoretical
Optical Properties Metric English Comments
Refractive Index 1.63
1.63
Component Elements Properties Metric English Comments
Al2O3 0.34 %
0.34 %
CaO 46.21 %
46.21 %
Fe2O3 0.77 %
0.77 %
K2O 0.050 %
0.050 %
Loss on Ignition(%) 0.050 %
0.050 %
MgO 0.38 %
0.38 %
MnO 0.16 %
0.16 %
SiO2 51.6 %
51.6 %
TiO2 0.050 %
0.050 %
Descriptive Properties Value Comments
Appearance White
Aspect Ratio (L/D) 20:1
Morphology Acicular
Copyright © lookpolymers.com All Rights Reserved