Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Nye Lubricants 718B (NG) Rheolube Grease

Category Fluid , Lubricant , Polyphenylether (PPE) Base , Silica Gellant
Manufacturer Nye Lubricants
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Nye Lubricants 718B (NG) Rheolube Grease.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Nye Lubricants.
Physical Properties Metric English Comments
Kinematic Viscosity at 40°C (104°F) 363 cSt
363 cSt
Base Oil; ASTM D445
Kinematic Viscosity at 100°C (212°F) 13 cSt
13 cSt
Base Oil; ASTM D445
Evaporation Loss 0.00 %
0.00 %
24 hrs, 150C; ASTM D972
Mechanical Properties Metric English Comments
Penetration P(0), 1/10 mm 191
191
ASTM D217
Oil Separation 1.0 %
1.0 %
24 hrs, 150C; FTM 719B, 321.2
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 260 °C
500 °F
Recommended
Minimum Service Temperature, Air 4.00 °C
39.2 °F
Recommended
Pour Point 4.00 °C
39.2 °F
Base Oil; ASTM D97
Descriptive Properties Value Comments
Base Fluid Type PPE
Gellant Type Silica (WL)
Users viewing this material also viewed the following: