Material Notes:
Description: Nylene® 9110 G43 is a 43% glass fiber reinforced specialty nylon.
Physical Properties Metric English Comments
Specific Gravity 1.42 g/cc
1.42 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 165 MPa
24000 psi
ASTM D638
Elongation at Break 20 %
20 %
ASTM D638
Flexural Modulus 10.3 GPa
1500 ksi
ASTM D790
Izod Impact, Notched 1.60 J/cm
3.00 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 221 °C
430 °F
ASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 203 °C
398 °F
ASTM D648