Material Notes:
High Impact Grade; Property data for dry as molded samples.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation.
Physical Properties Metric English Comments
Density 1.07 g/cc
0.0387 lb/in³
Linear Mold Shrinkage 0.0070 cm/cm
0.0070 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 51.0 MPa
7400 psi
ASTM D638
Elongation at Break 55 %
55 %
ASTM D638
Flexural Modulus 1.71 GPa
248 ksi
ASTM D790
Izod Impact, Notched 9.99 J/cm
18.7 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 254 °C
489 °F
ASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 68.0 °C
154 °F
ASTM D648